玻璃钢模塑格栅 38*38H30 (OFR-25)
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name Content
Type Resin
35% OFR-25、IFR-25、VEFR-25 Fiberglass 33%
E Filler 31%
ATH、PR Others 1% ---
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
| Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
| Fiberglass | 33% | E |
| Filler | 31% | ATH、PR |
| Others | 1% | --- |
Introduction of raw materials Resin type
Code Resin type Flame retardant property Standard color Recommended usage occasions MP-5 Phenolic type Oxygen index can reach about 80 Brown Low toxicity and high flame retardant, fire safety is very important for the occasion VEFR-25 Vinyl type Oxygen index 28 or above Grass green,Yellow, Grey, Orange Acid, alkali and other corrosive harsh environment VEFR-10 Vinyl type Oxygen index 35 or above Dark grey, Black Flame retardant requirements of high acid, alkali and good occasions IFR-25 Meta benzene Oxygen index 28 or above Grass green,Yellow, Grey A VEFR type economy, and excellent, moderate acid alkali and solvent IFGR-30 Benzene food grade Oxygen index 26 Yellow Mainly used in meat products and food processing plants OFR-25 Ortho type Oxygen index 28 or above Grass green,Yellow, Grey General acid and alkali environment OCR Ortho type Oxygen index below 28 Green,Yellow, Grey OFR-25 economy, no flame retardant requirements
Introduction of raw materials
Resin type
| Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
| MP-5 | Phenolic type | Oxygen index can reach about 80 | Brown | Low toxicity and high flame retardant, fire safety is very important for the occasion |
| VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
| VEFR-10 | Vinyl type | Oxygen index 35 or above | Dark grey, Black | Flame retardant requirements of high acid, alkali and good occasions |
| IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
| IFGR-30 | Benzene food grade | Oxygen index 26 | Yellow | Mainly used in meat products and food processing plants |
| OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
| OCR | Ortho type | Oxygen index below 28 | Green,Yellow, Grey | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code Coarse sand type Recommended usage occasions E Non alkali sand For high strength requirements and high corrosion resistance of the occasion
The type selection of coarse glass fiber
| Code | Coarse sand type | Recommended usage occasions |
| E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code Filler type Recommended usage occasions ATH Aluminum hydroxide Retardant, smoke suppression, corrosion-resistant occasions PR No filler, pure resin For high corrosion-resistant applications
Selected filler type
| Code | Filler type | Recommended usage occasions |
| ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
| PR | No filler, pure resin | For high corrosion-resistant applications |