PULTRUDED GRATING T-1810
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
| Name | Contect | Type |
| Resin | 25% | OFR-25、IFR-25、VEFR-25 |
| Fiberglass | 65% | E |
| Filler | 8% | ATH、PR |
| Others | 2% | --- |
Introduction of raw materials
Resin type| Code | Resin type | Flame retardant property | Recommended usage occasions |
| MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
| VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
| VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
| IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
| IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
| OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
| OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
| Code | Coarse sand type | Recommended usage occasions |
| E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
| Code | Filler type | Recommended usage occasions |
| ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
| PR | No filler, pure resin | For high corrosion-resistant applications |
Sand surface
Smooth surface
Antiskid groove surface
Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 18%
Approx Weight (With three-core shoots): 13.8kg/m²

Liner load(units:mm)
| Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
| (mm) | 300 | 500 | 800 | 1500 | 2000 | 2500 | Load |
| 400 | 0.4 | 0.67 | 1.07 | 2 | 2.67 | 3.34 | 5900 |
| 600 | 1.24 | 2.06 | 3.3 | 8.25 | --- | --- | 2300 |
| 800 | 2.76 | 4.59 | 7.35 | 13.8 | --- | --- | 2300 |
| 1000 | 5.16 | 8.6 | 13.8 | --- | --- | --- | 2200 |

Uniform load(units:mm)
| Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
| (mm) | 300 | 500 | 800 | 1500 | 2000 | 2500 | Load |
| 400 | 0.1 | 0.17 | 0.27 | 0.5 | 0.67 | 0.83 | 29600 |
| 600 | 0.46 | 0.77 | 1.24 | 2.32 | 3.1 | 3.87 | 12700 |
| 800 | 1.38 | 2.3 | 3.67 | 6.89 | 9.18 | 11.5 | 7300 |
| 1000 | 3.22 | 5.37 | 8.6 | --- | --- | --- | 4600 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories