Genius FRP    

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25、IFR-25、VEFR-25

Fiberglass

65%

E

Filler

8%

ATH、PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

 The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T5020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 50%

Approx Weight (With three-core shoots): 15.66kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

6000.250.51
0.761.272.294.57---
9000.761.271.783.36.112.2---
12001.522.293.566.613.527.2---
15002.543.816.3512.524.649.5---
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

6000.510.761.272.293.056.35---
9001.022.033.816.869.4------
12003.36.3512.5------------
15006.8613.5---------------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  