方管-间苯

方管-间苯

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Square tube

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Square tube

A*B*T1*T2


A*B*T1*T2


ST25A25*25*3.2*3.20.53

1" x 1" x 1/8" x 1/8"

1.17
ST25B25*25*6.4*6.40.9

1" x 1" x 1/4" x 1/4"

1.98
ST32A32*32*3.2*3.20.7

5/4" x 5/4" x 1/8" x 1/8"

1.54
ST32B32*32*6.4*6.41.24

5/4" x 5/4" x 1/4" x 1/4"

2.73
ST38A38*38*3.2*3.20.85

3/2" x 3/2" x 1/8" x 1/8"

1.87
ST38B38*38*5*51.25

3/2" x 3/2" x 3/16" x 3/16"

2.76
ST38C38*38*6.4*6.41.54

3/2" x 3/2" x 1/4" x 1/4"

3.4
ST44A44*44*3.2*3.21.01

7/4" x 7/4" x 1/8" x 1/8"

2.23
ST44B44*44*6.4*6.41.83

7/4" x 7/4" x 1/4" x 1/4"

4.03
ST50A50*50*3.2*3.21.14

2" x 2" x 1/8" x 1/8"

2.51
ST50B50*50*3.5*3.51.24

2" x 2" x 1/8" x 1/8"

2.73
ST50C50*50*4*41.42

2" x 2" x 3/16" x 3/16"

3.13
ST50D50*50*5*51.74

2" x 2" x 3/16" x 3/16"

3.84
ST50E50*50*6.4*6.42.12

2" x 2" x 1/4" x 1/4"

4.67
ST54A54*54*3.2*3.21.24

9/4" x 9/4" x 1/8" x 1/8"

2.73
ST54B54*54*4.8*4.81.78

9/4" x 9/4" x 3/16" x 3/16"

3.92
ST60A60*60*5*52.1

19/8" x 19/8" x 3/16" x 3/16"

4.63
ST64A64*64*3.2*3.21.48

5/2" x 5/2" x 1/8" x 1/8"

3.26
ST64B64*64*4.4*4.41.97

5/2" x 5/2" x 3/16" x 3/16"

4.34
ST64C64*64*6.4*6.42.8

5/2" x 5/2" x 1/4" x 1/4"

6.17
ST76A76*76*3.2*3.21.77

3" x 3" x 1/8" x 1/8"

3.9
ST76B76*76*5*52.7

3" x 3" x 3/16" x 3/16"

5.95
ST76C76*76*6.4*6.43.39

3" x 3" x 1/4" x 1/4"

7.47
ST76D76*76*9.5*9.54.89

3" x 3" x 3/8" x 3/8"

10.8
ST89A89*89*6.4*6.43.95

7/2" x 7/2" x 1/4" x 1/4"

8.71
ST101A101*101*3.2*3.22.38

4" x 4" x 1/8" x 1/8"

5.25
ST101B101*101*5*53.61

4" x 4" x 3/16" x 3/16"

7.96
ST101C101*101*6.4*6.44.61

4" x 4" x 1/4" x 1/4"

10.2
ST152A152*152*6.4*6.47.1

6" x 6" x 1/4" x 1/4"

15.7
ST152B152*152*9.5*9.510.4

6" x 6" x 3/8" x 3/8"

22.9
ST152C152*152*12.7*12.713.5

6" x 6" x 1/2" x 1/2"

29.8
STR2525*25*3.175*3.1750.7

1" x 1" x 1/8" x 1/8"

1.54

 Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face